Intertek Test Results
CTS Flange recently commissioned an independent report by Intertek to test the results for copper/steel assembly with and without an electrolysis insulator.
Results show that the CTS flange assembly with electrolysis insulator was able to withstand five times greater loading, with tripping time increased four fold.
Specimen | Dielectric Breakdown Voltage(kV) |
Time to Trip (Sec) |
Location of Failure |
---|---|---|---|
-001 Non-insulated Flange |
4 | 2.5 | Edge of Flange |
-002 Non-insulated Flange |
20 | 10.0 | Edge of Flange |